TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Wed, 7 Nov 2001 08:21:16 +0800
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (90 lines)
Hi, Mike,

How are you masking the stencil? From the top or the bottom? Too thick a
mask, especially on the bottom, will cause the stencil to deform and you'll
lose the gasketing of the stencil to the board. For low volume, the
simplest form of masking that works is Kapton tape on the top side. It's
thin and strong enough, and doesn't cause additional wear to the stencil.

If you paste a very fine pitch location but don't place a component, there
are no leads to "soak up" the solder when it melts. Particularly if the
pads are over-pasted (width), there is a greater tendency for bridging to
occur. If you have excessive stencil wear, then you're probably looking at
replacing the stencil soon anyway, so either consider omitting the QFP
pattern next time or reducing the aperture size.

Peter Duncan




                    Michael Bell
                    <Michael.Bell@        To:     [log in to unmask]
                    GPC.CO.NZ>            cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:              Aero/ST Group)
                    TechNet               Subject:     [TN] QFP Solder Pad  Shorts
                    <[log in to unmask]
                    RG>


                    11/07/01 07:13
                    PM
                    Please respond
                    to "TechNet
                    E-Mail Forum."






Hi all,

I have just come across a problem with a reflowed PCB that has a footprint
for a QFP on it, but no QFP placed.  It seems the footprint has paste
stenciled onto it, various other components placed, and then reflowed.
However, after reflow, it is notorious for having a number of solder
shorts.
We have tried masking off the apetures in the stencil to avoid depositing
paste on the pads, but I am noticing wear on the stencil.  Has anyone got
any ideas of what is causing the solder shorts between the pads, or how to
solve this???

Cheers

Mike

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2