Jason,
Is there a good reason why you don't remove the gold from the leads prior
to assembly? Can you put them through a solder pot before mounting them to
the board? Another possibility is to see if you can obtain the parts with
an alternative lead finish.
Peter Duncan
JASON CROSS
<jason.cross@AL To: [log in to unmask]
CATEL.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: Aero/ST Group)
TechNet Subject: [TN] Gold Embrittlement
<[log in to unmask]
G>
11/08/01 06:27
AM
Please respond
to "TechNet
E-Mail Forum."
Hello all,
I have a case that recently came up questioning possible gold
embrittlement in solder joints. I was wondering if I could bounce a few
numbers off this forum and see what all of you think. Any help or
reference material
would be great.
Ceramic 4 lead oscillator.
CuNiAu lead finish.
Component gold plating thickness specs are 12 to 40 microINCHES of gold.
(I realize that this is quite high)
Calculations indicate varying % gold by volume of solder to be between
1.36% and
2.28%, all the way up to possibly as high as 3.13%
Do you know what the acceptable gold volumes are and the impact to long
term reliability?
Increasing the volume deposited might only make the solder wick up
further along the lead, pulling more gold into the joint. This probably
wouldn't really help in this particular case.
Would increasing the pad size AND solder volume (hence trying to
minimize forcing solder up the lead but rather keeping it flat on a
larger surface) help? Would the gold spread evenly to the entire solder
volume or still concentrate near the lead?
Any help or reference material would be great!
Regards,
--
Jason Cross
Physical Technology Engineer
Alcatel Canada, Inc.
(613) 784-4793
(888) 662-3425 x 4793
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|