Shipley Bulge TesterHi Chuck,
as you seem to be a Siemens company, I assume that you are not performing plating operations yourselves, and so I would query your need to do bulge testing. The test requires that a sample is prepared by plating a specific thickness (normally greater than the normal thickness of plating) onto a backing sheet, peeled off and then tested. If you are not doing the plating process yourself, you will have problems making the sample, no?
Atotech also supply a bulge tester (or you could use them as a service ?)
Dougal Stewart
email: [log in to unmask]
phone: +44 1896 822204
mob: +44 7984 629667
----- Original Message -----
From: Brummer Chuck
To: [log in to unmask]
Sent: Wednesday, August 28, 2002 6:13 PM
Subject: [TN] Shipley Bulge Tester
Hi,
Does anyone know anything about the Shipley SE 800 Mechanical Bulge Tester?
I need to find one to test, rent or whatever. The Shipley web site was not very helpful.
We have a procedure that calls for this equipment.
Thanks in advance
Chuck Brummer
Acuson (A Siemens Co.)
818.734.4930
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|