In your car, you must have a defrost for you rear window. When the wire mesh
breaks, some garage uses a conductive paint or epoxy to repair the traces.
You might look into this at your local garage or windshield repair shop...
Good luck
Michel Arbour
Memotec Communication Inc.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Peter tremewen
> Sent: Thursday, May 31, 2001 2:28 AM
> To: [log in to unmask]
> Subject: [TN] Conductive Paint......
>
>
> Hi Techneters,
>
> The current discusion about Conductive epoxy brings to mind a
> question I had about conductive paint.
> Does any one know where I might find a good reasonably cheap
> source of conductive paint? The only source
> I have found here in Australia is prohibitively expensive, and
> not very conductive. Any sugestions would
> be appreciated. The aplication is but low voltage and low amps,
> and designed to be totally disposable if
> a fault occurs, so low cost is an important consideration.
>
> Thanks......
>
> )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O(
>
> The Sinister Dragon
>
>
> Hey, Just because I'm EVIL,
> Doesn't make me a bad person...... >:-)
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|