Peter, In your car, you must have a defrost for you rear window. When the wire mesh breaks, some garage uses a conductive paint or epoxy to repair the traces. You might look into this at your local garage or windshield repair shop... Good luck Michel Arbour Memotec Communication Inc. > -----Original Message----- > From: TechNet [mailto:[log in to unmask]]On Behalf Of Peter tremewen > Sent: Thursday, May 31, 2001 2:28 AM > To: [log in to unmask] > Subject: [TN] Conductive Paint...... > > > Hi Techneters, > > The current discusion about Conductive epoxy brings to mind a > question I had about conductive paint. > Does any one know where I might find a good reasonably cheap > source of conductive paint? The only source > I have found here in Australia is prohibitively expensive, and > not very conductive. Any sugestions would > be appreciated. The aplication is but low voltage and low amps, > and designed to be totally disposable if > a fault occurs, so low cost is an important consideration. > > Thanks...... > > )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( > > The Sinister Dragon > > > Hey, Just because I'm EVIL, > Doesn't make me a bad person...... >:-) > > ------------------------------------------------------------------ > --------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following > message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & > Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ------------------------------------------------------------------ > --------------- > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------