TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wenger, George M.
Date:
Thu, 16 Apr 2009 19:07:28 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (266 lines)
I think Dave was correct about the question marks a


Joyce,



I think Dave was correct about the question marks after "Authority" in

his  email.  Remember he's the lowly engineer fighting off the

alligators, trying to figure out how to convert from microns to inches

while he's looking for the light at the end of the tunnel.



Sorry Dave.  You do know I don't believe what I wrote above but I

couldn't pass up the opportunity.





Regards,

George

George M. Wenger

Andrew Wireless Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell]

[log in to unmask]

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman

Sent: Thursday, April 16, 2009 3:53 PM

To: [log in to unmask]

Subject: Re: [TN] NTC - [TN] Gold/Tin Intermetallics, why are we afraid?



Hi Joyce! Authority??????? I am just a lowly engineer trying to find the



light at the end of the tunnel without having all the alligators in the 

swamp get me first. My luck will be that the light at the end of the 

tunnel is Doug driving a train!



Dave







Joyce Koo <[log in to unmask]> 

Sent by: TechNet <[log in to unmask]>

04/16/2009 02:48 PM

Please respond to

TechNet E-Mail Forum <[log in to unmask]>; Please respond to

Joyce Koo <[log in to unmask]>





To

[log in to unmask]

cc



Subject

Re: [TN] Gold/Tin Intermetallics, why are we afraid?













Ha, the authority is spoken!



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman

Sent: April 16, 2009 3:32 PM

To: [log in to unmask]

Subject: Re: [TN] Gold/Tin Intermetallics, why are we afraid?



Hi Joyce - my response would "it depends" (and Doug gets another Diet

Mt. 

Dew) as Rockwell Collins utilizes immersion silver pwb surface finishes

on 

many IPC Class 3 type products with no reliability issues.



Dave







Joyce Koo <[log in to unmask]> 

Sent by: TechNet <[log in to unmask]>

04/15/2009 04:11 PM

Please respond to

TechNet E-Mail Forum <[log in to unmask]>; Please respond to

Joyce Koo <[log in to unmask]>





To

[log in to unmask]

cc



Subject

Re: [TN] Gold/Tin Intermetallics, why are we afraid?













"ImAG finishes have a 12-month shelf life in a controlled environment

(<35[degrees]C/<85[degrees] RH), which can be significantly shortened

when exposed to air pollution with high sulfur and chlorine content.

Silver embrittlement Embrittlement



A general set of phenomena whereby materials suffer a marked decrease in

their ability to deform (loss of ductility) or in their ability to

absorb energy during fracture (loss of toughness), with little change in

other mechanical properties, such  ([Ag.sub.3]Sn intermetallics) of

solder joints may occur when the finish thickness exceeds IPC-4553

recommendations and Pb-free, high silver content solders are used. ImAG

is not recommended for high-reliability assemblies that must meet

IPC-6010 Class 3 requirements, but is acceptable for Classes 1 and 2."



http://www.thefreelibrary.com/Will+discoloration+tarnish+ImAg+reliabilit

y%3F+Watch+for+silver...-a0193896272



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*

Sent: Wednesday, April 15, 2009 4:34 PM

To: [log in to unmask]

Subject: Re: [TN] Gold/Tin Intermetallics, why are we afraid?





 Hi Vlad,

I cannot comment on your specific case, but look at the pics below to

see 

Ag-embrittlement.

Sorry 'Netters, IPC strips pics.



Werner



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential 

information, privileged material (including material protected by the 

solicitor-client or other applicable privileges), or constitute

non-public 

information. Any use of this information by anyone other than the

intended 

recipient is prohibited. If you have received this transmission in

error, 

please immediately reply to the sender and delete this information from 

your system. Use, dissemination, distribution, or reproduction of this 

transmission by unintended recipients is not authorized and may be 

unlawful.



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask]

or 

847-615-7100 ext.2815

-----------------------------------------------------





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential 

information, privileged material (including material protected by the 

solicitor-client or other applicable privileges), or constitute

non-public 

information. Any use of this information by anyone other than the

intended 

recipient is prohibited. If you have received this transmission in

error, 

please immediately reply to the sender and delete this information from 

your system. Use, dissemination, distribution, or reproduction of this 

transmission by unintended recipients is not authorized and may be 

unlawful.



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask]

or 

847-615-7100 ext.2815

-----------------------------------------------------





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2