TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"West, Jim" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 8 Sep 1999 14:23:28 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Mike,

The board will be functioning in a controlled environment.

-----Original Message-----
From: Keel, Mike [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 1999 2:03 PM
To: 'TechNet E-Mail Forum.'; 'West, Jim'
Subject: RE: [TN] Board house repairing broken trace


Hi Jim

What kind of environment does the board have to function in ?

M Keel
San Diego



-----Original Message-----
From: West, Jim [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 1999 3:01 PM
To: [log in to unmask]
Subject: [TN] Board house repairing broken trace


Hi all,

I received a board that looks like the board house scratched the board and
broke a trace.  They made a repair and applied a clear and green mask over
the repair.  My question is how reliable is the repair?  What are the
possibilities the trace can be lifted over time?
The board tested ok as far a continuity goes.  Any input would be greatly
appreciated.

P.S.
The boards is an adapter board that is used for signal transfer.

Jim West
Manufacturing Engineer

[log in to unmask]                        PROMARK ELECTRONICS
ph. (614) 351-6216                               1909 Arlingate Lane
fax (614) 351-2180                                Columbus, OH 43228

<http://www.promark-us.com>   Promark Electronics Website

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2