TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Karen Tellefsen <[log in to unmask]>
Date:
Fri, 23 Jan 1998 09:13:59 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jerry Cupples <[log in to unmask]>
Subject:
From:
Jerry Cupples <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (46 lines)
Good morning, Karen; you said:


>1.  Electromigration requires DC voltages and currents.
>
>        a. AC voltages and and current will not cause
>           the electrodissolution of copper, silver,
>           tin or lead.  The only materials that corrode
>           with imposed AC (<~10 kHz). are amphoteric
>           materials, like aluminum.
>
>        b. AC voltage and currents will not allow the
>           the electrodeposition of any metal that I know.
>           The metal deposited during one half wave will
>           dissolved during the 2nd half wave.
>
>2.  Imposing a small AC voltage (5 to 50 mV) on top
>    of a DC voltage and looking at the resulting
>    small AC current is good way of studying
>    electrochemical reactions like dissolution and
>    deposition of metals.  The frequencies used range
>    from 1 mHz to 100 kHz.  Frequencies over 100 kHz,
>    such as RF, are not useful for looking at
>    electrochemical reactions because the chemical
>    kinetics of these reactions are too slow.

1) I _love_ that kind of talk.
2) Been waiting a long time for someone to techno-incinerate Graham Naisbitt.


thanks,


Jerry

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2