TECHNET Archives

February 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, lduso - Diamond-MT.com
Date:
Wed, 7 Feb 2018 17:59:33 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Yes, a coating will wick up the leads and cause connectivity issues. Once
it is cured/dried, that should not happen unless it is put back into a
liquid state due to solvent contact or high-heat.

Lloyd Duso
Plant Manager
Diamond-MT
(814) 535-3505
www.Diamond-mt.com

On Wed, Feb 7, 2018 at 5:17 PM, Jack Olson <[log in to unmask]> wrote:

> sorry for the long delay (and thank you for the responses)
> but as I was reviewing these posts I had another question:
>
> Have you ever heard of problems with conformal coating material wicking up
> the connector leads and causing intermittent connections?
>
> thanks again,
> Jack
>
>
> On Wed, 6 Dec 2017 14:09:46 -0500, lduso - Diamond-MT.com <
> [log in to unmask]> wrote:
>
> (..snip...)
> >It's up to me to decide how close to J1 to get with the coating. I once
> >coated the leads of all the fine-pitch connectors and the customer said
> >that was too close. The next customer will reject the work if I don't coat
> >the leads.
>
>
>

ATOM RSS1 RSS2