TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 7 Jul 1998 09:03:12 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
From:
"by Dr. Eden Chen XianSong" <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain
MIME-Version:
1.0
Parts/Attachments:
text/plain (84 lines)
     The adhesion of conductive epoxy is very much dependent on the pad and
     component terminal. The Au pad and Ag/Pd component terminal have the
     best adhesion. Most of conductive epoxy will experience resistance
     change under 85/85 test. Stencil printing is better than dispensing.
     Dispensing always have the tailing problem.

     Try the vendors of AlphaMetal and Sumitomo.

     Eden


______________________________ Reply Separator _________________________________
Subject: Re: [TN] ASSY: Thermally/Electrically Conductive Epoxy
Author:  Non-HP-MChan ([log in to unmask]) at HP-Singapore,mimegw51
Date:    7/6/98 11:55 PM


can't you provide an stencil aperture for the component underside and use solder
for that interconnection so as to not add a dispensing process to your process
flow...if done correctly, you should not have any intermittent
connections...some of the  problems with using conductive adhesives are CTE
mismatches, depending on the paste you may have issues with rosin residues,
forming adequate fillets around the component and probably most
important...rework!

Marcelo

        -----Original Message-----
        From:   Jan Satterfield [SMTP:[log in to unmask]]
        Sent:   Monday, July 06, 1998 11:30 AM
        To:     [log in to unmask]
        Subject:        [TN] ASSY: Thermally/Electrically Conductive Epoxy

        We have an RF component that contains a metal pad on the underside of
        the component that is soldered to a pad on the pwb.  After reflow we are
        getting intermittent connections.  I need to find a thermally and
        electrically conductive epoxy that I can use to bond the metal pad to
        the pwb and will then withstand the temperatures of reflow while the
        leads are soldered.  This epoxy will need to be applied with a dispenser
        due to high volume.

        Any suggestions or vendors that I might contact?

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
        For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
        ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
 in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2