TECHNET Archives

July 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=iso-2022-kr
Sender:
Subject:
From:
Young Hwan Ju <[log in to unmask]>
Date:
Thu, 12 Jul 2001 14:43:37 +0900
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (142 lines)
 $)C
-----  H8<[GQ   ;g6w : YoungHwan Ju/SimmTech ( 2001-07-12 02:47 PM ) -----

                    YoungHwan Ju    <v=E@N :        [log in to unmask],[log in to unmask]
                                    B|A6@N :
                    2001-07-12      A&8q :           Re: [TN] Checking scaled flow value of prepreg at the
                    01:57 PM             incominginspection.(Document link: YoungHwan Ju)





Dear Chuck
Thank you for your sincere advice.
Regarding prepreg I also know there are several properties such as R/F,
S/F, G/T, R/C, V/C.
Actually most of our prepreg suppliers provide above data through the
inspection report whenever they send materials to us.
The thing that I really would like to know is what property is the most
influential in controlling board thickness when we make multilayer board
among R/C, S/F, R/F or other thing?
And I think after buying mini-press, checking scaled flow value at the
incoming inspection is the labor loss.
If you work for PWB manufacturing company, Does your company also check the
scaled flow value at the incoming inspection?
If so or not , please tell me the reason.

Regards
Jay Ju




                    Chuck Brummer   <v=E@N :        [log in to unmask]
                    <cbrummer@ACUS  B|A6@N :
                    ON.COM>         A&8q :           Re: [TN] Checking scaled flow value of prepreg at the
                     9_=E@N :               incominginspection.
                    TechNet
                    <[log in to unmask]
                    RG>


                    2001-07-11
                    11:48 PM
                    "TechNet
                    E-Mail Forum."
                     ?!0T   H8=EGO?)
                     AV=J=C?@ .;
                    Chuck Brummer
                     ?!0T   H8=EGO?)
                     AV=J=C?@ .





 Buying the press for scaled flow is a wise idea.  There are many
parameters involved in
making and controling prepreg.  Just checking two, one of which is
subjective, is not
adequate.  Scaled flow testing will not always tell you what is wrong with
the prepreg but
will let you know that the product itself has some factor that is out of
spec.

Chuck Brummer
Acuson

Young Hwan Ju wrote:

> Dear all technetters
> I work for PWB manufacturing company which mainly produces multilayer
> board.
> When we inspect prepreg at the incoming material inspection, we just
check
> resin content & gel time.
> Now, we have the plan to buy mini-press for the purpose of checking the
> scaled flow value of prepreg at the incoming inspection
> Our hot pressing process engineer insists that just checking resin
content
> & gel time is not sufficient and ineffective to control the board
> thickness.
> I'd would like to know checking the scaled flow value at the incoming
> inspection is usual and effective way to control the board thickness.
> As long as I know, there are few of PWB manufacturing companies to check
> the scaled flow value at the incoming inspection.
> I have two questions.
>
> 1. To buy a mini-press is wise judgement for checking scaled flow value
at
> the incoming inspection?
> 2. At the incoming inspection, checking resin content & gel time is
> actually not sufficient and ineffective? If so why?
>
> Any remarks will be helpful for me
>
> regards
> Jay Ju
>
>
---------------------------------------------------------------------------------

> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
---------------------------------------------------------------------------------


---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2