TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 7 Oct 2005 08:46:18 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
"Victor G. Hernandez" <[log in to unmask]>
Parts/Attachments:
text/plain (178 lines)
I beg to differ, we use to put six 1" square raw board coupons in a
single mout and prep for grinding and polishing.   There out vendor with
at least 6 mounts on a fixture.   The biggest problem is either round
square or rectangular.   Size is the biggest PROBLE along with diameter
of wheel and consumables.   It is so much easier to have a personal
phone conversion that to type all dialogue.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.
Sent: Friday, October 07, 2005 8:30 AM
To: [log in to unmask]
Subject: Re: [TN] Microsection

Franklin,

I think the reason you didn't get any answers is because there is no one
out there that can put 3 PCB coupons in a single mount and hit the
center of 6 mil dia holes simultaneously.  That would require mounting
all three PCB coupons so that the holes line up.  My colleague (Pat) who
I consider a world class cross sectioner can put multiple PCB coupons in
a single mount and get close to the centers but not right at the center.
When we do multiple coupons in a single puck he grinds and polishes to
the center of first one that he gets to the center, we photograph it and
then continue to the next one.

The trick to getting very close to the centers on each coupon is to take
each PCB coupon in a small hand held vice and close the jaws just
outside of the PCB holes of interest and use the hardened jaws of the
vice as a stop and grind just until you break into the hole.  Do this
for each PCB sample and then mount the coupons in a single puck.  Since
you have broken into the perimeter and opened the hole you can easily
(if you use vacuum) fill the holes with mounting compound and you won't
have to grind much material away.  From what I've seen from Pat's talent
(or maybe it's his tricks) is the real key to grinding to where you want
to look is to minimize how much material needs to be ground away.


Regards,
George
George M. Wenger
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin Asbell
Sent: Friday, October 07, 2005 8:47 AM
To: [log in to unmask]
Subject: Re: [TN] Microsection

(chuckle) No, that thought hadn't hit me... So you're suggesting I
continue till I can hit a 6 mil hole with my shaky hands? Well okay,
I'll continue.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair K. Hogg
Sent: Friday, October 07, 2005 7:33 AM
To: [log in to unmask]
Subject: Re: [TN] Microsection

Franklin,

Have you considered that you may be a pioneer in what you are trying to
do and that no one here can offer any advice cause nobody has tried it
before?

Blair

>>> [log in to unmask] 10/07/05 07:02AM >>>
(chuckle)

Yes, can you believe it... got no response at all, now Steve, they
jumped all over his request, I'm thinking it has to do with his website
and he allowing people to post pictures, and so people want to keep him
happy...(laughing as people wonder how serious I am) luckily I'm past
that point where I would take it personal, but years ago....hmmm, well
anyway.

What I'm looking for is a device to grind/polishing a single mount (3 pc
board coupons in a single puck) by hand.

In days past I could do a somewhat decent job, with todays smaller
holes, even down past 10 to 8 and even 6 I find it difficult to hit the
center of the hole +/- 10%.

Beuhler makes what they call the PC-Met jr, selling cost $2500 for the
kit which is crazy as they sell the complete kit for 6 mounts at $4500.

So I'm looking for a used unit, or one from another source (not even
sure who else might make one, perhaps Struers)

So that's my need today...any suggestions would be wonderful.

Franklin


*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this email in error please notify the
system manager.

This footnote also confirms that this email message has been swept for
the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2