TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob METCALF <[log in to unmask]>
Date:
Thu, 2 Oct 2008 15:43:35 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Sean Hill <[log in to unmask]>
Subject:
From:
Sean Hill <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (161 lines)
Bob,

Try Palomar Technologies.
We just used them a couple of weeks and they did an outstanding job for
us.
They were able to perform the wire bonding and the pull strength
testing.
They generate a very professional report along with SPC and CPK data.


 Don Beck
Palomar Microelectronics
General Manager
Desk: (760) 931-3694
Cell:  (760) 208-0013
Fax:   (760) 931-5191
Web: www.palomartechnologies.com


Kind regards,
Sean Hill
Process Engineer
Cirexx International
Cell # 209-839-7495
E-MAIL [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob METCALF
Sent: Thursday, October 02, 2008 3:11 PM
To: [log in to unmask]
Subject: Re: [TN] Failure Analysis Lab with Ion Chromatography testing
capabilities

Is anybody aware of any U.S. lab that can do gold wire bonding testing?

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech

USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS
INFORMATION. 
Unauthorized disclosure and/or use of information contained in this
email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted
with 
it. 



"Stadem, Richard D." <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
10/02/2008 01:05 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Failure Analysis Lab with Ion Chromatography testing
capabilities






You may wish to contact Specialty Labs. I believe they have the
capability. They are in Minneapolis. They do a lot of work for us here
at GD, and I use them for failure analysis work for my consulting
engineering clients quite often. They do really good work, but cost
considerably less than other FA companies in the upper midwest area.
www.thespecialtylab.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Verrette
Sent: Thursday, October 02, 2008 1:22 PM
To: [log in to unmask]
Subject: [TN] Failure Analysis Lab with Ion Chromatography testing
capabilities

Can anyone recommend a good failure analysis lab with Ion Chromatography
testing capabilities?
 
We are in the Boston area.
 
Jim Verrette
Senior Electrical Engineer
 
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2