TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Fri, 23 May 2008 12:44:20 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (123 lines)
Another enigma where you won't know you're finished, until you're
finished.
Dewey


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Friday, May 23, 2008 12:17 PM
To: [log in to unmask]
Subject: Re: [TN] Methodology for determining the # of reworks ENIG
finished solder lands for leaded components can withstand

Joe, I have seen the "it depends" notes...............8-) 

........and of course they are correct, the finish, the re-work process,
the
component being re-worked will all contribute.

One thing though - how many times do you need to rework it for your
purposes? 

I have seen load board designs which were purposely build to withstand
many
(10+) rework operations on BGA's using enig as a finish (here the
component
could not be socketted for DVT testing purposes).

The issue there was actually not the enig, but how to keep the solder
resist
in place with a BGA design during multiple re-work in the "dog bone"
area
between the pad and the via.

If you need data on that contact me off line.

Have a great memorial day weekend Techies.............

John

 
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Macko
Sent: Friday, May 23, 2008 10:41 AM
To: [log in to unmask]
Subject: [TN] Methodology for determining the # of reworks ENIG finished
solder lands for leaded components can withstand

Techs,

 

I am looking for some help / guidance on how to analytically determine
the number of times the same leaded component can be replaced on a ENIG
finished board before the solder lands located on the PCB have been
degraded beyond their capability to provide a solderable class 3 surface
(.e., how many times can the ENIG finished solder lands with stand a
rework/component remove & replace).  I suspect the dissolution rates of
nickel and copper come into play however I am not sure how to approach
this issue and suspect there are some relatively straightforward
formulas out there to accomplish this task. Everyone has a different
idea and there are numerous rules of thumb discussed but I would like to
try something more analytical (without having to use a supercomputer).
Thanks again and everyone enjoy the long weekend.

 

Best Regards,

-joe

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2