TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 21 Oct 2008 11:35:19 -0400
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Content-type:
text/plain; charset=iso-8859-1
Subject:
From:
"Gumpert, Ben" <[log in to unmask]>
In-Reply-To:
Content-transfer-encoding:
quoted-printable
Parts/Attachments:
text/plain (37 lines)
From what I understand, using Pb-free BGAs and SnPb solder requires a reflow profile that stays slightly hotter (above 217°C) slightly longer to ensure the SAC reflows enough to mix adequately with the SnPb paste.

But I don't think there's enough test data available to make a strong conclusion on the reliability.

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster
Sent: Tuesday, October 21, 2008 11:21 AM
To: [log in to unmask]
Subject: [TN] Lead Free BGA'S

Our assembly house recently assembled some boards with Lead Free BGA's for us and when I asked them if they used a lead free process they responded with.

We use leaded solder (Sn63Pb37) with a hybrid oven profile to accommodate the lead-free BGA. I hope this answers your question. Please let me know if you have any more questions."
Is this a common process, is this a reliable process

Any input is appreciated

Thank You
John Foster


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2