Doug,
If you can not find the weighing boats you like, you might try to make them
yourself - subject to how many you need.
Get the thickest aluminum foil you can find at the store/supplier, 2-3X
layers if necessary, and form it over a mandrel of some nature [eg - a pine
furring strip, with rounded edges, or a suitable cardboard box]. Trim if
necessary.
May have to provide a carrier tray to move the filled tray to your oven,
etc.
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, January 21, 2010 12:01 PM
To: [log in to unmask]
Subject: [TN] aluminum weighing boats
Good morning all,
A quick question for the group. I am looking for a source of aluminum
weighing "boats", that would be about 4-6" long, 1-2" wide and maybe 1/2"
deep. Has to be aluminum because the application is high temp. Needs to
be disposable.
Most of the chemical or lab supply place that I normally use have aluminum
weighing pans/boats, but all are much smaller, usually 1-2" in diameter. I
need something larger.
Thanks.
Doug Pauls
Rockwell Collins
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|