TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 14 Aug 2007 18:28:49 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gerald Bogert <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Subject:
From:
Gerald Bogert <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
MIME-Version:
1.0
Comments:
RFC822 error: <W> MESSAGE-ID field duplicated. Last occurrence was retained.
Parts/Attachments:
text/plain (44 lines)
August 14, 2007

August 14, 2007

We have experienced this same issue.  We call it "sensuous" coating because
of the feel when you touch it.  This could be related to a specific
manufacturers coating (will not mention the brand name here), or incomplete
cure or improper mix ratio.  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Tuesday, August 14, 2007 3:05 PM
To: [log in to unmask]
Subject: [TN] Tacking potting material

What causes tacky polyurethane potting material? Is tacky a cause for
rejection or is it a cosmetic issue only?
Thanks in advance
Kat

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2