TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Creswick, Steven" <[log in to unmask]>
Date:
Thu, 15 Mar 2007 06:32:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain;charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
Thanks for the prompt reply. I can do the gold calculations - lots of
stuff on the tech-net telling me how to do that. We have not seen any
solderability issues. I would still like an explanation of the reasoning
behind the minimum nickel thickness( besides a keypad type application).
Regards Steve Kelly>

Steve,
>
> I will likely solder quite well, but the gold is quite thick for
> soldering to without incurring the wrath of gold embrittlement.  I would
> not be so concerned about the thin nickel as the overabundance of gold.
>
> If the gold were nice and soft, it would be nice for gold ball bonding!
> But, the nickel is quite thin.
>
> If the numbers are correct, you did not receive ENIG - have them sent
> back
>
> Steve C
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
> Sent: Wednesday, March 14, 2007 9:31 PM
> To: [log in to unmask]
> Subject: [TN] IPC ENIG SPECIFICATION
>
> Hi All,
> I  have a question about this specification. Obviously when the
> technical
> gurus wrote this they had good reasons for specifying the nickel at a
> minimum of 118 microinches. One of our customers recently received some
> parts from the far east. The print called for ENIG but the parts came in
> with approx. 20 microinches of nickel and approx. 40 microinches of
> gold.
> My question is what are the reliability/solderability concerns on low
> nickel. Thanks in advance. Regards Steve Kelly
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT
> FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY
> FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are
> not the intended recipient, you are hereby notified that any review,
> distribution, or copying of this communication is strictly prohibited.  If
> you have received this communication in error, please immediately notify
> the sender by return e-mail, and delete this e-mail message and any
> attachments from your computer.
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2