TECHNET Archives

August 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Fri, 6 Aug 2010 21:16:25 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gabriela <[log in to unmask]>
Subject:
From:
Gabriela <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<007501cb3590$4d82eda0$e888c8e0$@com>
Content-Type:
text/plain; charset="windows-1255"
MIME-Version:
1.0
Parts/Attachments:
text/plain (131 lines)
Yes, Dave is right. I had them too and had fun popping the big ones.
See that the leads which are at the ends of the part-look like mounting
spacers- don't have this defect because they are from a different batch of
leads and are OK.
There is a big chance that leads with this defect would have been OK for
through hole mounting and would have passed without detection of the plating
with excess of organic brighteners .
Gaby

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: е 06 аевеси 2010 20:54
To: [log in to unmask]
Subject: Re: [TN] blumpy

Hi Chris!

Looks just like what I had back in Tulsa. I started calling what I saw
"Blumpy" (bumpy + lumpy = blumpy) ;^)

http://stevezeva.homestead.com/files/Connector_Blumpies.jpg

Dave Hillman and a few others said that it was co-deposited organics from
bright tin plating.

To me, the solder joints in the picture look like "head-in-pillow" joints. I
wouldn't accept them and I would reject the parts back to the vendor. The
part looks like a TI part. I thought TI was plating their leads with
palladium and not tin though...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Friday, August 06, 2010 1:35 PM
To: [log in to unmask]
Subject: [TN] blumpy

So a customer has the blumpies (see link to pictures below).  The hand (dry)
solder melt-front smokes like a freight train under the microscope.

My questions are:

Have we really coined "blumpy"? and
If it wets and forms proper fillets, is it conformant?

Thanks!
Chris


This message contains attachments delivered via ShareFile.
 - 30910 as soldered.jpg
 - 30910 heel as recvd.jpg

Download the attachments here -
https://robisan.sharefile.com/d-TEMP-80276654fa1bea874e093013e1b
-----------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

__________ Information from ESET NOD32 Antivirus, version of virus signature
database 5347 (20100806) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com


 

__________ Information from ESET NOD32 Antivirus, version of virus signature
database 5347 (20100806) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com
 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2