Parts/Attachments:
text/plain (20 lines)
Hi Scott,
Your concern is proper--I take it you want to put this CBGA onto FR-4.
While your CBGA is small, the small pitch will result in very short solder
joint heights. Depending on the delta-T's experienced in operation and the
design life, you may or may not meet design goals. You certainly can get some idea
from IPC-D-279, but that is for Sn63 and similar solders; no generally
applicable model exists for any of the LF-solders as yet.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2