Steve Kelly <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
Steve,

I echo what Joe has already said.  This amount of gold should not be a
problem for gold wire bonding unless the components have not attained
bonding temperature (on the order of 150C), or something is moving/softening
during bonding.

Even aluminum wire should bond well to this amount of gold - but also as Joe
indicated, the long term reliability may be of some question.

See if the Customer can share a bit more info with you as to the type of
bonding performed, temperatures, and the type of problems experienced.

Steve Creswick - Gentex

-----Original Message-----
From: Steve Kelly [mailto:[log in to unmask]]
Sent: Saturday, June 22, 2002 11:22 AM
To: [log in to unmask]
Subject: [TN] Wire bondable gold


We made some flex circuits for a customer and wound up putting too much gold
on - approx. 75 microinches. The nickel is averaging 153. The gold meets all
the purity specs. Under the wire bond area is a large heat sink. My customer
is having difficulties wire bonding. Is too much gold a problem or can the
heat sink cause issues. Regards Steve Kelly
--------------------------
Sent from my BlackBerry Wireless Handheld (www.BlackBerry.net)

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2