TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Mon, 24 Jun 2002 09:11:29 +0200
MIME-Version:
1.0
X-To:
Bev Christian <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Ingemar Hernefjord (EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (45 lines)
Hi Bev,
saw once that a crack must never be longer that the size of the solder grain size. As soon as the crack exceeds that size, it's a presumptive danger. Sounds a bit of an exaggeration to me, but  have seen that expression more than once.
Ingemar Hernefjord
Ericsson Microwave Systems



-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: den 20 juni 2002 21:33
To: [log in to unmask]
Subject: [TN] cracks in solder joints


Hopefully this will start off a nice discussion.  I have kept it general for
that purpose.

Shades of voids in BGAs...   How big of a crack in thermally cycled solder
joints is too big of a crack?

Bev Christian
Research in Motion

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2