TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 18 Mar 2008 10:35:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Igoshev, Vladimir" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
From:
"Igoshev, Vladimir" <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Of causea, as it's sitting on the pad.



Regards,



Vladimir



----- Original Message -----

From: TechNet <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Tue Mar 18 10:30:07 2008

Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability



In Mask defined BGA pads; is the mask surface higher than the BGA pad surface?  



-----Original Message-----

From: TechNet [mailto:[log in to unmask]]On Behalf Of Thayer, Wayne

Sent: Tuesday, March 18, 2008 7:20 AM

To: [log in to unmask]

Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability





Buy any BGA built on glass composites and turn it over under a microscope.  You will see mask defined pads.

 

Xilinx is the biggest purveyor of "do as I say, not as I do".  In their guidelines, they insist, using the logic Vladimir puts forth, that non-mask defined pads are superior.

 

We usually work with small balls.  The "weak link in the chain" with these is the adhesion of the pad to the laminate, not cracks in the solder.  Kyocera did a pretty decent study on this a few years ago, and concluded that the most robust designs used mask defined pads.

 

The big problems with mask defined pads are mask contamination on the pads and poor solder mask resolution on behalf of most pcb fabricators.  If the fab can do a good job on the mask, you will get stronger, more uniform as-reflowed balls.

 

Maybe the big parts work totally different from my small ones, but I have not seen any problems with mask defined pads other than those stated above.

 

Wayne Thayer



________________________________



From: TechNet on behalf of Igoshev, Vladimir

Sent: Tue 3/18/2008 9:18 AM

To: [log in to unmask]

Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability







There is a very short answer: Fracture Mechanics :-)



When we have an SMD pad, there is an unavoidable stress concentration in

the vicinity of the triple junction "solder/solder pad/solder mask".



Non-SMD pads are free from that kind of stress concentration, as they

are "wrapped up" with solder.



Regards,



Vladimir



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Kirk, Graham (GE

EntSol, Intelligent Platforms)

Sent: Tuesday, March 18, 2008 8:06 AM

To: [log in to unmask]

Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability



Hi Joyce,



I realize that CTE mismatch is responsible for the fatigue, I am trying

to understand why the solder mask has so much effect on the solder

joint.



Graham Kirk



Senior Technologist



Radstone Embedded Computing



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo

Sent: 18 March 2008 11:07

To: [log in to unmask]

Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability



Fatique, due to CTE mismatch or poor design.  My 1st guess.

Jk

--------------------------

Sent using BlackBerry





----- Original Message -----

From: TechNet <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Tue Mar 18 06:18:08 2008

Subject: [TN] Solder Mask Defined Pad BGA Reliability



Hi All,















Can anybody tell me what the actual mechanism is that propagates cracks

in the device to ball joint on plastic BGA's (Leaded balls) with SMD

pads under thermal cycling?















Graham Kirk







Senior Technologist







GE Fanuc Intelligent Platforms Ltd









---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential

information, privileged material (including material protected by the

solicitor-client or other applicable privileges), or constitute

non-public information. Any use of this information by anyone other than

the intended recipient is prohibited. If you have received this

transmission in error, please immediately reply to the sender and delete

this information from your system. Use, dissemination, distribution, or

reproduction of this transmission by unintended recipients is not

authorized and may be unlawful.



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------







---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------




ATOM RSS1 RSS2