Hi Ken,
Another, more precise, method is laser ablation. With special lasers you can
remove the soldermask and do it only and rather exactly where you want this
done. (the hand/Dremel/eraser method is probably cheaper, but more of a pain
in the you-know-where and less precise.)

We have saved a number of very expensive boards that way and removed only
the mask off the copper area that had to be soldered. It leaves you with a
clean copper area and a small 'ditch' around the pad where ablation removed
some of the FR4.
Contact me off-line.

Regards,
Ahne Oosterhof,
A-Laser, Inc.,
Beaverton, OR.
503-641-9428




-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ken Patel
Sent: Tuesday, June 29, 2004 16:41
To: [log in to unmask]
Subject: [TN] Soldermask on PTH pad???
Importance: High

Technetters,

We have pads of hand soldering locations covered with solder mask making it
difficult to solder. Is there any other way to solder besides scarping the
solder mask (abrasive) and use solder fountain? I am looking for any easy
way to remove solder mask or soldering technique.

Any help will be highly appreciated.
Re, Ken Patel

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2