I have to analyze failures of a subassemblies of our subcontractor. As cause
of problem I suppose cracks/voids in the prepreg (of a16-layer pcb), caused
either by poor siloxane-treatment between glass and epoxide - or - because
crushing of prepreg integrity by microlocal mechanical stress during the pcb
press operation. As cause of this stress I assume following: During the
press operation the prepreg conforms to the bounds formed by the laminate
and their conductors at both sides. Between the walls/shoulders ot two
buried vias the prepreg will be pressed, the resin will flow away, but the
glass will be squeezed. I think glass fibres squeezing together can resulte
to resin recession.
But let me tell you some details: The failing subassemblies I've to analyze,
contains transformer windings which are implemented as a 16-layer pcb. The
winding shows dielectric breakdown between different winding layers (and
sometimes between different windings on the same layer). This breakdown
happens after some hours run-in at 120°C and 500VDC (500VDC as test voltage,
failures also at lower tension at at AC) .Before them, all pcb has passed
successful a hi-voltage test at ambient temperature.
The diel. strength for the closest distance of 65mm prepreg should be around
2.5kV, or a little bit less because IPC-2221, § 4.1.2, not 500V!
I tend to see any loss of the electric strenght of a laminate/prepreg as
function of the temperature, the hi-temp aging, and material defects.
The occuring pcb temperature of 120°C seems in accordance with IPC-2222, §
4.3. So I'm looking for material defects, especially cracks: if cracks span
a part of
the 65mm (prepreg), the electric strenght will decrease, because the
electric strenght of a cracks (like air) amounts 1kV/mm (instead of 40kV/mm.
Hope to get some engelnotes.
Bernhard
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|