TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 20 Nov 2006 13:20:28 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"David D. Hillman" <[log in to unmask]>
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (103 lines)
Hi Joe - Your statement......." type AR or type UR does not coat the BGA
solder balls/solder connections located under the BGA so you are violating
the acceptability requirements in IPC-A-610" has me some confused. What
IPC-A-610 requirement is violated?

Dave Hillman
Rockwell Collins
[log in to unmask]




             "Macko, Joe @
             IEC"
             <joe.macko@L-3COM                                          To
             .COM>                     [log in to unmask]
             Sent by: TechNet                                           cc
             <[log in to unmask]>
                                                                   Subject
                                       Re: [TN] BGA and conformal coating
             11/20/2006 12:47
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               "Macko, Joe @
                   IEC"
             <joe.macko@L-3COM
                   .COM>






Vered,

I would start with IPC-A-610 and J-STD-001 documents. One item that is over
looked is that spraying a board with for example type AR or type UR does
not
coat the BGA solder balls/solder connections located under the BGA so you
are violating the acceptability requirements in IPC-A-610!

Good luck,
- Joe


-----Original Message-----
From: Vered BS [mailto:[log in to unmask]]
Sent: Monday, November 20, 2006 8:40 AM
To: [log in to unmask]
Subject: [TN] BGA and conformal coating

looking for reviews/articles or case studies regarding conformal coating on
BGA
for military/aerospace environment
Appreciate any comment or sharing your experiance
Thanks
Vered

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2