TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=us-ascii
Old-Return-Path:
Date:
Mon, 16 Jun 1997 15:45:16 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Tue Jun 17 11:
44:35 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/13440
TO:
Return-Path:
<TechNet-request>
Status:
O
X-Loop:
Resent-Message-ID:
<"KXToF.0.G8Q.EFQfp"@ipc>
Subject:
From:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wdiVr-000BkPC; Mon, 16 Jun 97 15:36 CDT
X-Lotus-Fromdomain:
LEXMARK@LEXMTA
>From willli Mon Jun 16 15:
37:12 1997
Message-Id:
Parts/Attachments:
text/plain (22 lines)

We purchased a Pace PRC 2000 unit to repair solder on gold.  Using this
unit we remove the solder and re-plate the area with gold.  It is a fairly
tedious process and uses some pretty harsh chemicals but seems to work well
for us.  E-mail me direct at [log in to unmask] if you would like some more
information.

Andrea Shurtz
Lexmark Contract Manufacturing


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2