We purchased a Pace PRC 2000 unit to repair solder on gold. Using this unit we remove the solder and re-plate the area with gold. It is a fairly tedious process and uses some pretty harsh chemicals but seems to work well for us. E-mail me direct at [log in to unmask] if you would like some more information. Andrea Shurtz Lexmark Contract Manufacturing *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************