Dear Mr. Werner,

The wave soldering parameters are as follows. As indicated earlier this is a 2.4mm thick board

CONVEYOR SPEED -- 110 CM/MIN
ZONE 1 -- 100  C
ZONE 2 -- 110  C
ZONE 3 -- 120  C
SOLDER TEMP -- 250  c

We are also trying to get the flux parameters which we feel is critical.

Hope this will give more clarity. Kindly give your feedback

Rgds

pradeep

[log in to unmask] wrote at Wed Jul 15 09:20:05 GMT+05:30 2009:
>Dear Mr.Werner,
>
>They claim, they did bake it at 120degC for 2 hours before they were wave soldered. Will moisture affect solderability ? Can you kindly brief how. We were under the impression that it affects only the PTH reliability. 
>
>regards
>
>pradeep
>
>Werner Engelmaier /* wrote at Wed Jul 15 01:25:30 GMT+05:30 2009:
>> Hi Pradeep,
>>Did they bake the moisture out of the PCBs prior to wave soldering?
>>Werner
>>
>>
>> 
>>
>>
>> 
>>
>>-----Original Message-----
>>From: mp3 <[log in to unmask]>
>>To: [log in to unmask]
>>Sent: Tue, Jul 14, 2009 6:50 am
>>Subject: [TN] Solderability
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>Hi,
>>
>>We are a PCB manufacturer and we had supplied some 2.4mm thick PCBs to one of 
>>our customers who has complained regarding solderability issue. They say there 
>>are having issues with respect to blowholes / pinholes after wavesoldering. We 
>>had checked for solderability on the coupon and had ensured that everything is 
>>acceptable prior to the despatch. We repeated the same after receipt of the 
>>feedback and found the results to be OK. To simulate it, we sent a couple of 
>>bare circuits to a 3rd party assembler and got it wave soldered. The hole 
>>diameters are 2.55mm and 1.0mm . The photographs after wavesoldering trials are 
>>attached. We find it to be quite OK. We feel that since there are no components, 
>>and since the diameter is on the higher side, there will be a slight depression 
>>at the centre. But the customer insists that the trial boards too have a 
>>problem. Can you give a feedback on this after checking the attached 
>>photographs. We were asking our customer to check on the parameters like fluxing 
>>etc. And he says all are well in control. Any inputs to understand this issue 
>>better.
>>
>>rgds
>>
>>pradeep
>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to 
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
>>additional information, or contact Keach Sasamori at [log in to unmask] or 
>>847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>
>>
>> 
>>
>>
>>
>>
>>
>>
>>
>>-------------------------------
>>Micropack Ltd, Bangalore, India
>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to 
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
>>additional information, or contact Keach Sasamori at [log in to unmask] or 
>>847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>
>>
>> 
>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>
>>
>


-------------------------------
Micropack Ltd, Bangalore, India

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2