TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sun, 13 Feb 2000 20:57:35 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Jon Moore <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
In a message dated 1/27/00 3:26:59 PM US Eastern Standard Time,
[log in to unmask] writes:

<< Has anyone out in wave soldering land tried using a wave soldering fixture
 that allows you to change the rotation of the board so that the edge of the
 board isn't parallel to the conveyor?

 I'm told that rotating the board slightly (say 5 degrees - not 90 degrees!)
 can reduce the
 occurrence of solder skips on SMT chips (caps and resistors).  Any
 experience out there to confirm or deny this?
  >>
I have tried such a fixture and had relatively good success.  Part of the
cause was poor design layout, yet this was a mature product with no budget
available for a new layout.  EMC makes a standard wave solder pallet with a
rotatable inner piece that can be set to any angle, and it worked well.

Jon Moore

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2