TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 22 Feb 2000 01:22:12 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Jon Moore <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
In a message dated 2/10/00 2:24:28 PM US Eastern Standard Time,
[log in to unmask] writes:

<< ."What are the best "cleaning solutions" (chemicals) to use which are
 most effective for removing the flux residuals from PWB's that also has
 compatibility with a wide variety of different chemicals and materials such
as
 adhesives, connectors, sleeving, wire, inks, epoxies and etc.?"  >>
The best that I have seen so far is called Aquasonic and it is made by JNJ.
For those that cannot use a water based cleaning process, Prozone from
Multicore also did quite well in my tests.

Jon Moore

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2