TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Rob Strecker <[log in to unmask]>
Date:
Mon, 13 Aug 2007 16:39:06 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (65 lines)
Rob:

There are three possible causes of your foam problem.

First, we assume that fluxes cause foam when they dissolve into an aqueous cleaner... that is a good first assumption.
The cleaner is supposed to repress/kill the foam.. but, it needs to be warm enough to do that.. if you are not up to recommended temperature, that could be the problem...

Second, the defoaming capacity of any cleaner is finite, and if you are overloading with flux, you are overwhelming this capacity.   (Do you get foaming from the start, or only after cleaning for a long while?)

And, last, you simply may not have enough foam killing capacity in your cleaner.

The obvious, and probably likely least acceptable solution is to add defoamer..

Rudy Sedlak
RD Chemical Company

Rob Strecker <[log in to unmask]> wrote: All,

Has anyone else had foaming issues in an aqueous wash batch cleaner?
What are some of the causes of excess foaming?  We are applying our wave
flux via spray; however this flux is also suitable in foaming flux
applications.  We are currently in the process of optimizing our flux
application in the wave to significantly reduce the flux residue on the
boards.  This includes optimizing the sprayers, preheats and dwell time.
Initial tests show this is not having a major impact in reducing the
foaming.  We will be testing boards with only SMT flux residue, then
ones with only wave flux residue.  The theory is that by themselves they
do not foam but when mixed cause foaming.  We have recently changed
Paste suppliers, thus we now have two different manufactures of flux
mixing in the wash (one from SMT, one from wave).  Could this be a cause
of excessive foaming?

 

Thanks,

Rob Strecker


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


       
---------------------------------
Park yourself in front of a world of choices in alternative vehicles.
Visit the Yahoo! Auto Green Center.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2