Dan,
sounds like a case for ceramic substrates, like Alumina or Aluminum
Nitride (AlN). Extremly low CTE, inert to humidity, rigid, cheap and can
be processed by several american companies. And if they need
multilayers, you can give them LTCC. E.g.
http://www.mskennedy.com/store.asp?pid=7943&catid=19680
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Skweres
Sent: den 13 augusti 2007 21:25
To: [log in to unmask]
Subject: [TN] Another Request.
Fellow Technetters,
I have another request from a customer that I do not have an immediate
answer(s) for. Once again I was hoping that with the wealth of knowledge
you collectively have that perhaps you could assist me in assisting my
customer. They need a circuit board that...
a.. Will reside within a float assembly of a gyroscope.
b.. The environment will consist of hydrogen with trace helium.
c.. A concern is the moisture absorption or adsorption, the
hygroscopic properties, of the circuit materials used in the stackup.
They're searching for materials with extremely low coefficients of
hygroscopic expansion and contraction, CHE and CHC. The board needs to
maintain stable electrical, mechanical and dimensional properties. Is it
generally better to go with a rigid design rather than a flex design
when concerned with the affects of ambient moisture?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|