Steve,
The only issues I'm aware of would be the quality of the plating process
(e-copper). But this would also be true plating 1oz onto 3oz.
We routinely plate up 2oz on 2oz and we monitor this process throughout.
As with all e-plating processes, control control control is the key
Franklin Asbell
Steve Collins wrote:
>
> Are there any reliability concerns in requesting a 4 oz board to start with
> 2oz base material and plate up the extra 2 oz with plated copper over
> starting with 3 oz base material and plating 1 oz for a 4 oz finished
> product.
>
> At this point I'm not as interested in comments on price since I realize
> the cost difference and availability issues involved here.
>
> Steve Collins
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|