Once upon a time the bare board house I used to work for was making a 4 oz.
finished board. We tried plating 2 oz. up to 4 oz. We were not able to get
our plating uniform enough to produce a consistent 4 oz. copper surface.
Take if from someone who has been there; do whatever you have to in order to
get 3 oz. material to start with.
Russ Bafford
Sovereign Circuits
330-538-3900
-----Original Message-----
From: Steve Collins <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, July 21, 2000 4:56 PM
Subject: [TN] 3 oz material
>Are there any reliability concerns in requesting a 4 oz board to start with
>2oz base material and plate up the extra 2 oz with plated copper over
>starting with 3 oz base material and plating 1 oz for a 4 oz finished
>product.
>
>At this point I'm not as interested in comments on price since I realize
>the cost difference and availability issues involved here.
>
>Steve Collins
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|