Hi Scott,

Two options I would suggest looking into
        Equipment Upgrade for a selective spray fluxer if you don't already
have one.  It only puts flux where you want it and you can control how much.
        A mask (custom made) to block areas that don't need flux.  They're
cost effective for large volume part numbers since the masks can be
expensive.  My old Hollis wave flow machine used pallets so it was just an
extra piece that hooked into it.  I imagine there are ways of doing without
the pallet - finger conveyor.  Now if I only had my notes to give you a
lead.

I was looking into both options before leaving my last job so I didn't get a
chance to actually try them.

Hans

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Process Engineer
Toppan Electronics, Inc.
770 Miramar Road
San Diego, CA 92126
(858) 695 - 2222 ext. 241
(858) 695 - 6823 fax
[log in to unmask]


-----Original Message-----
From: Rougeux, Scott [mailto:[log in to unmask]]
Sent: Monday, April 02, 2001 12:28 PM
To: [log in to unmask]
Subject: [TN] Flux Deposition


Good Afternoon,

I am wondering what approaches are available for measuring the amount of
flux applied to the bottom side of a circuit card using a spray fluxer...or
for that matter any type of flux application method.

Thanks in advance,

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2