Hi linda. The answer is "No". No Black Pad, but Brittle Fracture is well possible.
Regards,
Vladimir
SENTEC
------Original Message------
From: Linda Langley
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: Linda Langley
Sent: Sep 18, 2009 06:12
Subject: [TN] Black Pad
I know we have had this subject many times before so I did go to the
archives and still can't find an answer. My question, is Black Pad only
associated with ENIG? Is it possible with immersion Tin?
Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca