TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 16 Sep 2009 16:07:31 +0000
Reply-To:
Subject:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Content-Type:
text/plain
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Hi Lee,



What do you mean by "overheated"? The structure of the solidified solder shouldn't depend on how high it was heated above liquidus,



I have pictures of SAC 305 after very long aging at rather high temperatures (they were published a while ago), so if you need them please let me know.





Regards,



Vladimir

SENTEC 

------Original Message------

From: Lee Whiteman

Sender: TechNet

To: [log in to unmask]

ReplyTo: TechNet E-Mail Forum

ReplyTo: [log in to unmask]

Sent: Sep 16, 2009 11:36

Subject: [TN] SAC-305 IMAGE



Does anyone have a cross-section image of SAC-305 that has been

overheated (i.e. solder iron was kept on too long or the thermal profile

was too high)?



If so, please ship it over to me in a JPG format. I have to show some

people what it looks like.



Thanks.



Lee Whiteman, PMP

Senior Member Engineering Staff

L-3 Communications East

Telephone: (856) 338-3508

FAX: (856) 338-2906

E-Mail: [log in to unmask]

 



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------







SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca


ATOM RSS1 RSS2