Hi Werner,
Good seeing you again at APEXPO.
I heard at the show of one company whose returns for lead-free products are
running 3% higher than those produced with traditional solders. With razor
thin margins for many products, that is a lot. The remake doubles the cost...
good money after bad.
Fortunately, there is a long standing, reliable and truly environmentally
friendly solution for making good solder joints and it is ready to step in when
lead-free falls on its face. :-)
The green-washing of lead-free as an environmentally friendly solution is,
IMHO, one of the really sad chapters of this industry's otherwise great
history.
All that was needed was for the politicians to listen to the scientists and
not the self-serving, ill-informed lobbyists.
And so it goes....
Very best,
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|