TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Craig Hillman <[log in to unmask]>
Date:
Wed, 27 Jun 2001 19:40:32 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (75 lines)
Craig

VP reflow has a severe disadvantage: the Fluorinert or Galden or
whatever, are amongst the world's worst global warmers, with a GWP of
about 10,000 and an atmospheric residence time of about 10,000 years.
This means that they leave a terrible legacy for the next 25 generations
or so. They are also targeted in the Kyoto Protocol for the same reason.
This means in rough figures that 2 kg of the stuff is equivalent to all
the CO2 a medium sized car (~2.5 litre engine) will produce during its
whole lifetime. The process is still used a large extent in Europe.

Perfluorocarbons should be used ONLY where there is absolutely no other
choice and under the maximum non-emissivity, in my opinion.

Brian

Craig Hillman wrote:
>
> Werner brings up an interesting point. Does anyone have an opinion on the
> trends in solder reflow in the contract assembly industry? Are we seeing a
> resurgence in vapor phase? Has flowing nitrogen during infrared fallen to
> the wayside? Interested in seeing your responses.
>
> Best Regards,
> Craig
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
> Sent: Thursday, May 31, 2001 1:19 PM
> To: [log in to unmask]
> Subject: Re: [TN] AW: [TN] Pad in Via for BGA's - Part II
>
> Hi Rush,
> Vapor phase soldering was and is thew most elegant engineering solution to
> soldering--no over-temperatures, no profiles, absolute temperature
> uniformity. What killed this approach in the past was inadequate
> equipment--thhis is no loger a problem.
>
> Werner Engelmaier
>
> ----------------------------------------------------------------------------
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ----------------------------------------------------------------------------
> -----
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2