TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Thu, 9 Sep 2010 10:57:05 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (252 lines)
Totally agree.  
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Thursday, September 09, 2010 10:16 AM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Hand Soldering

"Supported by Test Data" 
Some key features of the Standard and the appendix have heritage from the
use of rosin flux and abandoned Mil Standards. These have produced commonly
held and occasionally erroneous conclusions. 

Another thread here discusses "funded custodians". Who are the funded
custodians now? How are they qualified to shape the standards? What are the
implications? 

We, the staff at R&D, have experience with materials that pass J-standards
and TM-650 tests to be classified REL0. These materials perform very well in
certain service environments. However, they do not behave like Rosin. So, in
other service environments they do not perform as well as one might expect,
some might consider it poor performance.

In the end, the user of the flux must understand the material properties,
and as needed, communicate same to the end user. I have concluded, perhaps
unfairly, that the J-STD classifications and the TM-650 tests may not reveal
these important material properties. Leaving the manufacturing engineer with
a false sense of security and confidence.

What are the properties of the raw flux? 
What are the properties of the processed flux?
What is "processed" flux? 
What are the properties of the flux after an attempt to remove the residue? 
What are the properties of the flux after exposure to a humid service
environment (which BTW is quite unlike a clean environmental chamber)?
What are the properties of the flux after exposure to a condensing
environment? 

I submit that the TMs attempt methodize answers some of the above, while
others are not addressed.
In short all L0 fluxes are not going to perform equally in all service
environments. 

This complex issue confounded committee efforts to provide a simple answer. 

Guy



-----Original Message-----
From: Robert DeQuattro [mailto:[log in to unmask]] 
Sent: Tuesday, September 07, 2010 4:10 PM
To: TechNet E-Mail Forum; Guy Ramsey
Subject: RE: [TN] Hand Soldering

With regard to industry standards, J-std-001 D (in transition to E),
3.3, provides some guidance on the use of flux, particularly for Class
3.  Also, J-std-004 B provides greater information.  It appears that the
big issues with flux are related to their corrosive and conductive
properties, and ultimately determine the extent of cleaning required.
Ideally all supported by test data.

Bob

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Tuesday, September 07, 2010 3:03 PM
To: [log in to unmask]
Subject: Re: [TN] Hand Soldering

We use water soluble fluxes exclusively. But, I beg to differ. One must
be
very fussy. It is not a messy process, but, it much easier to have the
result look very good and still bite you with latent defects. 

For solder training, absolutely. No mess no fuss. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, September 07, 2010 2:24 PM
To: [log in to unmask]
Subject: Re: [TN] Hand Soldering

I totally agree!

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Linda Langley
Sent: Tuesday, September 07, 2010 11:15 AM
To: [log in to unmask]
Subject: Re: [TN] Hand Soldering

Ken,
Go with water soluble, hot water rinse, no mess no fuss!!

Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenneth Wood
Sent: Monday, September 06, 2010 8:30 AM
To: [log in to unmask]
Subject: [TN] Hand Soldering

Hi all.
What is the best setup for hand soldering as far as solder / cleaner?
Rosin core? Water soluble? No-Clean?
What cleaner too?

I've been using rosin core with various cleaners but I have a hard time
with
the white residue the cleaners leave.

Thanks
Ken





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2