Unfortunately Bev, it is definitely not "black pad." Totally random pads
completely or partially fail to wet leaving blob of solder on apparently
clean gold surface - we see this on small BGA lands and 1206 lands
Thanks
> -----Original Message-----
> From: Bev Christian [SMTP:[log in to unmask]]
> Sent: Tuesday, November 28, 2000 1:14 PM
> To: 'TechNet E-Mail Forum.'; 'Burtt, Nigel'
> Subject: RE: [TN] Ni/Au solderabilty
>
> Nigel,
> When you say random, how random? Does it appear to mainly happen to small
> pads connected to large pads elsewhere on the boards? If so, read up on
> black pad syndrome in the TechNet archives.
>
> regards,
> Bev Christian
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|