Dear TECHNETers,
It is my first post to this list, please forgive me if I ask an already
posted question, but I could not find any answer to my problem.
We have received, populated and soldered a set of 50 boards which have
voids in the gold plating layer into holes (either PTH and via holes). We
have discovered the problem because of a poor vertical fill of the holes at
wave soldering.
Is there any standard for this parameter ? Neither IPC nor PERFAG mention
anything about this, they just state on copper plating.
Is there any risk of corrosion in the future for these boards ? (they will
be installed in factories, means in "standard" environnement in terms of
humidity and temperature )
If yes, how would you prevent it ? ( we cannot post solder the holes,
because of the large quantity of these and also because many of them are
hidden under SMD part; I would personnaly would use conformal coating)
Many thanks for your help and kind regards
Marie Magnin
QA Manager
FIRSTEC SA
Rue du Grand Pré 70
CH 1211 Genève 2
Tél : +41(0)22 918 36 85
Fax : +41(0)22 918 36 93
mailto:[log in to unmask]
http://www.firstec.ch
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|