A few thoughts on this subject:
1. lay-up operator should sort and count layers to be laminated before
beginning each lay-up to be sure they have the correct amount of each layer.
2. then, when lay up is finished all layers should be used up. If not, this
is a clue that a layer has been left out. (or if short, an extra layer has
been used in a panel).
3. The final check is to measure each panel after lamination for correct
thickness. An incorrect lay-up will fall outside of the control limits of
the lot and should alert the operator to take action.
Phil Dam
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|