Hi, Paul,
If I were give the choice, I know which option I would go for - the QFP.
Board space required to locate the QFP and its associated fan-out is
greater, but if the design can afford the real estate, go for it.
Points in favour are:
- No need to X-ray in order to inspect joints
- More 'flexible' than BGA's (better strain relief), therefore more
resistant to creep fatigue.
- No need to underfill (if you do).
- PCB Flatness criteria not quite so vital.
- Rework is quicker and cheaper (especially if BGA is underfilled)
- Fewer long-term reliability issues (no cracked balls, if you'll pardon
the expression)
- Thermal profiling is easier.
- etc.
Points against:
- QFP's take up more board space than BGA's.
- They don't self-align as well as BGA's do during reflow.
Peter
"Black, Paul" <[log in to unmask]> 07/03/2003 07:22 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to "Black, Paul"
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] BGA vs. QFP
Hi Technetters,
Up until now, I have been spoiled in that the only BGA that I have had to
deal with had a 1.25mm pitch. Now, for a new design, Engineering is giving
me an option of a 64 pin BGA or QFP. Both have a pitch of 0.5mm; is the
consensus to stick with the BGA? Are there any potential gotcha's?
Thank you,
Paul Black
Manufacturing Engineer
Kronos
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|