Matt Byrne(Hadco) related experience with fungus in brightener as a
nodule source.

Timothy Gaylor reports nodules of smaller size.

QUESTIONS FOR THESE GENTLEMEN AND THE GROUP:

Wouldn't a polarity shift with unrectified or rippled current cause
nonuniform plating conditions whereby the brightener (or something else)
could be occluded?  Could this change in crystalline habit result in a
nodule?

[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2