TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Burke <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Wed, 29 Oct 2008 15:19:39 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (91 lines)
Wonder whether those nice people at the EU worked out how to solder to
aluminum using anything lead free??

Can it be done?

John Burke

(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Dixon
Sent: Wednesday, October 29, 2008 2:17 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering to Aluminum?

Sounds funny.  The flux is "compliant", but they suggest that you use it
with tin/lead solder.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, October 29, 2008 10:35 AM
To: [log in to unmask]
Subject: Re: Soldering to Aluminum?

Pete,

Seems to me there was recent thread here on something similar.  We have
soldered to stainless steel and I think the process is similar for
aluminum.  It has to do with the flux used.  Word of caution... I
believe it is an acid based flux so how it is applied and washed off may
be of concern.

From McMaster-Carr website:

Aluminum Soldering Flux

Use this paste flux with aluminum solder and any tin/lead solder to
solder aluminum and aluminum alloys. Also for use with copper, chrome,
and brass. Meets DOD 1866 and is ROHS compliant.
4-oz. Jar 7696A2   Each   $9.65
1-lb. Jar 7696A1   Each   $30.41

 I have not tried it.

Phil Nutting


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Houwen
Sent: Wednesday, October 29, 2008 10:01 AM
To: [log in to unmask]
Subject: [TN] Soldering to Aluminum?

Has anyone tried soldering lead free to an Aluminum circuit on
polyester?

We are looking at a very simple one component circuit that needs to be
on a material with some flexibility.  We do run millions of feet of
aluminum on polyester passive circuits in one of our plants.  I am being
asked to see if we can take advantage of the in house production to save
some cost.

My other thought is to just try a conductive adhesive, but we might need
to do some tooling for that, as this would require about 3 million of
these circuits/year.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2