Peter,
We have research papers here at Rockwell from 1990, stemming from an
incident we lovingly call "The Great Post Coat Massacre of 1990", which
show conclusively that conformal coating mascarading as an underfill is a
REALLY bad idea.  Unfortunately, I cannot release that paper to the public.
Since you cure from the outside in, underfilling a component with conformal
coating means you will have entrapped solvent in the centermost portion of
the component.  Bad karma there.  You do not get a uniform material that is
uniformly cured throughout the bulk, as you do with an underfill.

Doug Pauls
Rockwell Collins

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2