TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 2 Nov 2006 12:11:46 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Corey A Peterson <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="big5"
From:
Corey A Peterson <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Irving,



I've have been through several fluxes so far. Your best bet is something 

with a small amount of rosin to give the flux enough time on the wave. 

Currently I have a water based no-clean flux with a small amount of rosin 

that is working real well on test boards.   With regards to trying other 

surface finishes.  There was a paper at SMTAI 06 that mentioned SnCuNi as 

a surface finish and it  had similar erosion traits as SnPb you might want 

to look into that but you would have to weigh the issues.



Best regards,



CP





To:     <[log in to unmask]>, <[log in to unmask]>

cc: 



Subject:        RE: [TN] Copper Dissolution



Corey,



Thanks. It is very worth recommendation. What kind of flux type you 

recommend ?

ENIG is not allowed by our customers, we may need to try other finishing 

types .



Irving



-----Original Message-----

From: Corey A Peterson [mailto:[log in to unmask]] 

Sent: Thursday, November 02, 2006 11:55 PM

To: TechNet E-Mail Forum; Lee, Irving (§õ©ú©ô TAO)

Subject: Re: [TN] Copper Dissolution





Irving , 



There are several options here. 



1) Use an ENIG surface finish

2) Use a flux that is a bit more aggressive probably will need some rosin 

to give it enough legs" to last in the wave that long.  Avoid using the 

chip wave if possibly.  You are going to be hard pressed to find a flux 

that will last that long thru the wave solder pot. 

3) Specific minimum copper thickness for the knee 

4) Change solder pot to a less aggressive solder alloy 

5) Use the best thermal mitigation strategies and where possibly use 

bigger annular rings. 



Corey Peterson 







Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond 

to [log in to unmask] 



Sent by:        TechNet <[log in to unmask]> 



To:        [log in to unmask] 

cc: 



Subject:        [TN] Copper Dissolution 



 

How to avoid copper dissolution during lead free wave soldering ?



[1] Printed Circuit Board Size : 13"x16" , Thickness : 0.93"

[2] Lead Free  Solder Bar Type : SAC = Sn + 3 % Ag + 0.5 % Cu [3] Both 

sides Reflow prior to Wave Soldering [4] Wave time : 6 sec , Temperature : 

265 degree C





Irving Lee



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] 

or 847-615-7100 ext.2815

-----------------------------------------------------















This message (including any attachments) contains confidential 
and/or proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on 
the contents of this information is strictly prohibited and may 
constitute a violation of law.  If you are not the intended 
recipient, please notify the sender immediately by responding to 
this e-mail, and delete the message from your system.  If you 
have any questions about this e-mail please notify the sender 
immediately.

ATOM RSS1 RSS2