A question from a colleague of mine. Subject: Water soluble flux rinse
water.

What is the minimum water cleanliness level of the final rinse for
assembled/soldered PCB?

*That depends a great deal on what you are cleaning and how clean do you
want to get the substrate?  I have found that the best cleaning comes from
deionized water.  I generally consider RO water to be 100 kilohm-cm up to
about 1 megohm-cm and DI water to be above 1 megohm-cm.

Doug Pauls
Rockwell Collins

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2